1.4541 AISI 321 stainless steel equivalent

Dec 16, 2025

Залишити повідомлення

What is 1.4541 material ?

1.4541 is a V2A stainless steel stabilized with titanium, also known as AISI 321, Alloy 321, BS 321S31, BS 321S51, and X6CrNiTi18-10, exhibiting good corrosion resistance (PREN value 17.0 to 19.0). This material is non-magnetic (relative magnetic permeability μr < 1.3) and can be used at temperatures up to 550 ℃. In the solution annealed state (at room temperature +AT), it is widely used in industries such as the automotive industry, mechanical engineering, and the chemical industry.

1.4541 Material

What material is 1.4541 equivalent to?

Steel Grade Comparison Table|AISI / EN / GOST / DIN / JIS / GB The 1.4541 grade is the equivalent grade in the European (EN) standard to the commonly used American (AISI) 321 stainless steel, also known as UNS S32100, X6CrNiTi18-10, and SUS321 in the Japanese standard.

AISI 321 / UNS S32100
1.4541 / X6CrNiTi18-10
321S31
SUS321
0Cr18Ni10Ti
X6CrNiTi18-10

 

1.4541 Stainless Steel Chemical Composition (% by weight)

<= 0.08
<= 1.00
<= 2.00
<= 0.045
<= 0.030
17.0 – 19.0
9.0 – 13.0
>= 5 × C

 

1.4541 Stainless Steel  Mechanical Properties (at room temperature)

Standard Requirement (EN 10088-2)
520 – 720 MPa >= 520 MPa
Yield Strength (Rp0.2) >= 210 MPa >= 210 MPa
Elongation (A5) >= 40% >= 40%
<= 200 <= 200
~7.90 g/cm³ -

 

What is the difference between 1.4541 and 1.4301 material?

1.4301 stainless steel is low carbon chromium nickel stainless and heat resisting steel somewhat superior to Type 302 in corrosion resistance. 1.4541 stainless steel is known as stabilized grades of stainless steel, is Chromium nickel steel containing titanium.

 

What is the difference between 1.4541 and 1.4571 material?
The main difference is that 1.4541 (AISI 321) is a titanium-stabilized stainless steel based on 1.4301 (AISI 304), while 1.4571 (AISI 316Ti) is a molybdenum-containing 1.4404 (AISI 316L) grade that is also stabilized with titanium. This means 1.4571 has additional molybdenum for enhanced corrosion resistance, making it a better choice in chloride-rich environments, while 1.4541 is a more basic, cost-effective option for high-temperature applications where molybdenum is not critical.

 

GNEE currently has SUS 321 (UNS S32100) products in stock, including: plates, sheets, coils, strips, tubes, bars, and wires. In addition, we offer a variety of surface finishes for you to choose from, such as: No.1, 2B, 2D, BA, No.3, No.4, HL, No.8, sandblasting, etc.
We guarantee 100% quality. We will never deliver any defective products to our customers. Please contact us to customize your required product specifications, including shape, condition, surface treatment, and processing technology.Email: sales@gneestainless.com

SUS 321 stainless steel pipe
SUS 321 stainless steel pipe
SUS 321 stainless steel shim plate
SUS 321 stainless steel shim plate

Послати повідомлення